MIL-DTL-81736B(AS)
the leading end of the third production tape. If these two specimens pass, all production tapes
are satisfactory. If one or both of these specimens fail, the second and third production tapes are
unsatisfactory. A 15-foot specimen shall then be taken from the leading end of the second
production tape and the trailing end of the third production tape in order to determine if the first
and fourth production tapes are satisfactory.
4.5.2.3.4 Test result IV. If the last specimen leaving the loom run is the only one that fails
the strength test, the third and fourth production tapes are the only tapes in doubt. A 15-foot
specimen shall be taken from the trailing end of the fourth production tape and tested. If this
specimen passes the strength test, the third and fourth production tapes are satisfactory. If the
specimen fails, the fourth production tape is unsatisfactory. A 15-foot specimen shall then be
taken from the leading end of the fourth production tape in order to determine if the third
production tape is satisfactory.
4.5.2.3.5 Test result V. If the first and second specimens fail the strength test, a 15-foot
specimen shall be taken from the trailing end of the second production tape and the leading end
of the third production tape.
4.5.2.3.5.1 Case I. If one or both test specimens 2T and 3L pass the strength test, the third
and fourth production tapes are satisfactory. A 15-foot specimen shall then be taken from the
leading end of the first production tape and tested. If this specimen passes, the first and second
tapes are satisfactory. If this specimen fails, the first production tape is unsatisfactory and the
second production tape is in doubt. A 15-foot specimen shall be taken from the trailing end of
the first production tape to determine if the second production tape is satisfactory.
4.5.2.3.5.2 Case II. If one or both test specimens 2T and 3L fail the strength test, the
second and third production tapes are unsatisfactory. The first productions tape shall be tested
by taking a 15-foot specimen from the leading ends of the first and second production tapes.
Both specimens shall pass the strength test in order for the first production tape to be
satisfactory. The fourth production tape shall be tested by taking a 15-foot specimen from the
trailing end of the third production tape.
4.5.2.3.6 Test results VI. If the second and third specimens fail the strength test, a 15-foot
specimen shall be taken from the trailing end of the second production tape and the leading end
of the third production tape.
4.5.2.3.6.1 Case I. If specimens 2T and 3L pass the strength test, the first and second
production tapes are satisfactory and third and fourth production tapes shall be tested by taking a
15-foot specimen from the trailing end of the fourth production tape. If this specimen passes the
strength test, the third and fourth production tapes are satisfactory. If the specimen fails the
strength test, the fourth production tape is unsatisfactory and a 15-foot specimen then shall be
taken from the leading end of the fourth production tape in order to determine if the third
production tape is satisfactory.